UPM Institutional Repository

Dielectric characterization of thermoplastic natural rubber/strontium titanate composites at 10 Hz to 1 MHz


Citation

Hassan, Jumiah and Rajaram, Deventharan and Hashim, Mansor and Ahmad, Azizan and Abbas, Zulkifly (2008) Dielectric characterization of thermoplastic natural rubber/strontium titanate composites at 10 Hz to 1 MHz. Jurnal Fizik Malaysia, 29 (3&4). pp. 67-70. ISSN 0128-0333

Abstract

The dielectric properties of Thermoplastic Natural Rubber (TPNR)/Strontium Titanate (SrTiO3) composites was determined at room temperature, 27oC using the Impedance Analyzer at frequencies 10 Hz to 1 MHz. TPNR is formed as the matrix while SrTiO3 acts as the filler. Six samples were prepared at percentages of fillers from 0 to 50% at 10% intervals. The results indicate that the dielectric constant is almost independent of frequency from 100 Hz to 1 MHz, but the dielectric loss factor decreased with increasing frequency. This could probably be due to interfacial polarization and ionic losses. The dielectric properties are also affected by the composition of the filler, SrTiO3.


Download File

[img]
Preview
PDF (Abstract)
Dielectric characterization of thermoplastic natural rubber.pdf

Download (83kB) | Preview

Additional Metadata

Item Type: Article
Divisions: Faculty of Science
Publisher: Malaysian Institute of Physics
Keywords: Dielectric characterization; Thermoplastic natural rubber; Strontium titanate composite
Depositing User: Nurul Ainie Mokhtar
Date Deposited: 18 Jun 2015 06:26
Last Modified: 17 Sep 2015 00:56
URI: http://psasir.upm.edu.my/id/eprint/14045
Statistic Details: View Download Statistic

Actions (login required)

View Item View Item